Aluminum Anode Sled
Aluminum Anode Transport Platform: A robust solution for stable performance in electrolytic environments, offering precise voltage control and high efficiency.
Description
This aluminum pyramid anode is specifically engineered for the replacement of worn-out anodes on established offshore installations. Its installation is swift and straightforward, requiring a simple lowering onto the seabed. This efficient method of attachment not only saves time but also significantly reduces costs compared to alternatives like underwater welding. As a result, our anode sled proves to be the perfect solution for retrofitting anodes on subsea equipment and platforms.
Fabricated from high-purity alloys with minimal iron content, our anode sled meets the stringent standards set by ISO, NACE, and DNV.
Element | GALVALUM III | DNV-RP-B401-2011 | GS EP COR 201 |
---|---|---|---|
Zinc (Zn) | 2.0% ~ 6.0% | 2.5% ~ 5.75% | 4.75% ~ 5.75% |
Indium (In) | 0.01% ~ 0.02% | 0.015% ~ 0.04% | 0.015% ~ 0.02% |
Silicon (Si) | 0.08% ~ 0.2% | 0.12% max. | 0.06% ~ 0.12% |
Iron (Fe) | 0.13% max. | 0.09% max. | 0.12% max. |
Copper (Cu) | 0.006% max. | 0.003% max. | 0.003% max. |
Cadmium (Cd) | — | 0.002% max. | 0.002% max. |
Total Impurities | 0.1% max. | 0.1% max. | 0.1% max. |
Aluminum (Al) | Remainder | Remainder | Remainder |
This aluminum anode sled maintains stable performance in seawater and electrolytes with chloride ions due to its operational voltage being controlled within the range of -1.05 to -1.10 volts concerning the saturated calomel electrode (SCE).
Technical Measurement | Performance |
---|---|
Open Circuit Voltage (-V) | 1.10 min. |
Closed Circuit Voltage (-V) | 1.05 min. |
Current Capacity | 1135 A.h/lbs (2500 A.h/kg) |
Current Efficiency | 90% min. |
Consumption Rate | 7.6 lbs/A·y (3.4 kg/A·y) |